Catalyst is mixed with Resin or Top Coat to a ratio of 1% to 3% per lvolume.
Thus, mix 10ml catalyst in hot water to 30ml in cold water per 1L Top Coat or Resin to activate hardening process.
R325,00
Delivery will be Calculated at CheckoutCatalyst is mixed with Resin or Top Coat to a ratio of 1% to 3% per lvolume.
Thus, mix 10ml catalyst in hot water to 30ml in cold water per 1L Top Coat or Resin to activate hardening process
Catalyst is mixed with Resin or Top Coat to a ratio of 1% to 3% per lvolume.
Thus, mix 10ml catalyst in hot water to 30ml in cold water per 1L Top Coat or Resin to activate hardening process.